Dear all expert,
i have problem with gasket that used for cryogenic service. i used GASKET, FLAT RING: RF FLANGE: SIZE 24IN; CLASS 600LBS; MATL EXPANDED GRAPHITE WITH WIRE REINFORCE. the problem is, gasket always fail/leak during shutdown-start up Plant.

Please share to me another material gasket for cryogenic service else graphit material and asbestos material