Hi, can anybody tell me how can I see on the material cert. if the material is also usefull into the EU ? the material has been made in Japan, and refers only to the ASTM. and the material manufacturer has been certified acoording iso 9000.
 
I'm not aware that there is a certain type of material certificate necessary for products used in the EU. The problem you might have is that your client will not accept certificates with ASTM references if your documentation towards your client lists ISO numbers. For what do you need the certificates? For internal use only or do you have to present them to your client?
 
micalbrch, Thanks for your reply, this material is part of a new boiler, so the mat.certs have to be submitted to our client on the end. and they have to be accepted by the PED requirements.
 
Aah, okay! That is a completely different background and yes, that can be a problem. My recommendation is the start a new post (with the PED background info) in the Boiler and Pressure Vessel Engineering forum. I beleive that you will get some valuable answers there.
 
The PED plus it's guidelines will tell you what you need, or what you're 'required' to handover in case of a NoBo.

Mostly EN 10204 3.1 certs, maybe some 2.2 certs for bolting.

The cert's thus have to be EN 10204 3.1 (if it's a pressure vessel in cat I or higher acc PED).

PS: certs handover to client may be contract-mandatory, but PED is compulsory by legislation. NoBo will accept things, not the PED.
 
please note that if the material is to be used in PED cat. III or IV, the certificate shall be 10204-3.2 If the supplier has a quality system specificly for the fabrication/supply of the applicable material that is approved by a European competent body it may be a 10204-3.1 certificate.
 