gblackwo
Mechanical
- Apr 29, 2015
- 4
Hey everyone,
I've stumbled across these forums several times over the years, but this is the first time I've felt the need to make an account. I've found the threads here abundantly helpful lately, so thank you to everyone.
I'm upgrading a design of LP fired burner coils that are ordinarily ASTM A53 carbon steel 3/4" SCH80. The customer wants to run brackish water (6000mg/L) through the burners and suggested upgrading to 316SS. The coils are thermostatically limited to 180F, but this is the water temperature, and I expect that some portions of the coils do exceed this. The operating pressure of the coils range from ~370 psi at the inlet to ~180 psi at the outlet.
From the data I've seen, we would be operating in a range where pitting would easily occur in 316SS. I am wondering if 2205 would suffice for the coils. I am also trying to limit corrosion as much as possible by using CPVC in the system where possible and trying to get the customer to provide clean water for regular automatic system flushes.
Thank you.
I've stumbled across these forums several times over the years, but this is the first time I've felt the need to make an account. I've found the threads here abundantly helpful lately, so thank you to everyone.
I'm upgrading a design of LP fired burner coils that are ordinarily ASTM A53 carbon steel 3/4" SCH80. The customer wants to run brackish water (6000mg/L) through the burners and suggested upgrading to 316SS. The coils are thermostatically limited to 180F, but this is the water temperature, and I expect that some portions of the coils do exceed this. The operating pressure of the coils range from ~370 psi at the inlet to ~180 psi at the outlet.
From the data I've seen, we would be operating in a range where pitting would easily occur in 316SS. I am wondering if 2205 would suffice for the coils. I am also trying to limit corrosion as much as possible by using CPVC in the system where possible and trying to get the customer to provide clean water for regular automatic system flushes.
Thank you.