Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Tek-Tips community for having the most helpful posts in the forums last week. Way to Go!

Material costs

Status
Not open for further replies.

doorf

Chemical
Nov 14, 2002
7
0
0
US
Hi,

I'm looking for the costs of materials which will be used for tanks. The materials are SS304, Carbon steel, Aluminum, Fiber reinforced plastic and pyrex plexiglass. Can anyone guide me about these prices or where I can find the unit material costs as well as the cost of making vessels from these materials.

Thanks







 
Replies continue below

Recommended for you

hi doorf,
you can obtain the cost of these materials from Coulson& Richardson's-chemical engineering volume 6.
I have the cost in 1992,but i think the cost vary from that day .
304 1600bound/tonne
carbon steel 300 bound/tonne
aluminium 900 bound/tonne
 