Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Material database 2

Status
Not open for further replies.

ctopher

Mechanical
Jan 9, 2003
17,506
I am updating my material database.
If anyone would like to add materials, please let me know and I will try to add.
It would help me save time if you have the material specs, and an image of the material, if you have it.
You can download the file from my site below.
Thanks,

Chris
SolidWorks 07 3.0/PDMWorks 07
AutoCAD 06
ctopher's home (updated 03-13-07)
 
How about some cast aluminum materials:
C355=.101 density
A356=.097 density

Wrought aluminum material:
2014=.101

Low Alloy Steel materials:
4130=.283 density
4140=.283 density
4340=.283 density

and other miscellaneous materials:

Leaded Bronze=.326 density
Carbon=.056 density

All above materials are commonly used in aerospace designs



Macduff [spin]
Colin Fitzpatrick
Mechanical Design Engineer
Solidworks 2007 SP 2.2
Dell 390 XP Pro SP 2
nVida Quadro FX 3450/4000



 
Oh...and a star for you for supporting us SW users, and for having a cool website.

Best,

Macduff [spin]
Colin Fitzpatrick
Mechanical Design Engineer
Solidworks 2007 SP 2.2
Dell 390 XP Pro SP 2
nVida Quadro FX 3450/4000



 
Thanks Colin.
I will look into those mtls.
[cheers]

Chris
SolidWorks 07 3.0/PDMWorks 07
AutoCAD 06
ctopher's home (updated 03-13-07)
 
Colin,
Can you be more specific on the Carbon?
Thanks

Chris
SolidWorks 07 3.0/PDMWorks 07
AutoCAD 06
ctopher's home (updated 03-26-07)
 
Chris,
I'll have to get back to you on that. It's been awhile since I worked with carbon. I think just a generic grade. What did you find?

Macduff [spin]
Colin Fitzpatrick
Mechanical Design Engineer
Solidworks 2007 SP 2.2
Dell 390 XP Pro SP 2
nVida Quadro FX 3450/4000



 
pdybeck,
What do have available in carbon?

You know you guys.........we're going to have to take Chris out for a steak dinner for working on this. Oh......and for some beers too!

Macduff [spin]
Colin Fitzpatrick
Mechanical Design Engineer
Solidworks 2007 SP 2.2
Dell 390 XP Pro SP 2
nVida Quadro FX 3450/4000



 
Colin,

Carbon steels (and some stainless to boot)

STEEL ROUND BAR, ELASTUF PENN CF
STEEL ROUND BAR, ELASTUF A-2 HR
STEEL ROUND BAR, ELASTUF A-2 HR
STEEL ROUND BAR, ELASTUF A-2 HR
STEEL ROUND BAR, ELASTUF A-2 HR
STEEL ROUND BAR, ELASTUF A-2 HR
STEEL ROUND BAR, ELASTUF PENN HR
STEEL ROUND BAR, ELASTUF PB HR
STEEL ROUND BAR, A36 HFS
STEEL ROUND BAR, A36 MILD HR
STEEL ROUND BAR, 1010 HR
STEEL ROUND BAR, 1010 CD
STEEL ROUND BAR, 1017 CD
STEEL ROUND BAR, 1017 HR
STEEL ROUND BAR, 1018 CD STRESS RELIEVED
STEEL ROUND BAR, 1018 CD STRESS RELIEVED
STEEL ROUND BAR, 1018 CD STRESS RELIEVED
STEEL ROUND BAR, 1018 CD STRESS RELIEVED
STEEL ROUND BAR, 1018 CFS
STEEL ROUND BAR, 1018 CFS
STEEL ROUND BAR, 1018 HR AS-ROLLED
STEEL ROUND BAR, 1018 HR NORMALIZED
STEEL ROUND BAR, 1018 HR ANNEALED
STEEL ROUND BAR, 1020 HR
STEEL ROUND BAR, 1040/42/45 HR AS-ROLLED
STEEL ROUND BAR, 1040/42/45 HR NORMALIZED
STEEL ROUND BAR, 1040/42/45 HR ANNEALED
STEEL ROUND BAR, 1040/42/45 CFS
STEEL ROUND BAR, 1040/42/45 CFS
STEEL ROUND BAR, 1117 HR AS-ROLLED
STEEL ROUND BAR, 1117 HR NORMALIZED
STEEL ROUND BAR, 1117 HR ANNEALED
STEEL ROUND BAR, 1117/11L17 CFS
STEEL ROUND BAR, 1117 CD STRESS RELIEVED
STEEL ROUND BAR, 1117 CD STRESS RELIEVED
STEEL ROUND BAR, 1117 CD STRESS RELIEVED
STEEL ROUND BAR, 1117 CD STRESS RELIEVED
STEEL ROUND BAR, 1137 CFS
STEEL ROUND BAR, 1141 CFS
STEEL ROUND BAR, 1141 HR AS-ROLLED
STEEL ROUND BAR, 1141 HR NORMALIZED
STEEL ROUND BAR, 1141 HR ANNEALED
STEEL ROUND BAR, 1144 CD STRESS RELIEVED
STEEL ROUND BAR, 1144 CD STRESS RELIEVED
STEEL ROUND BAR, 1144 CD STRESS RELIEVED
STEEL ROUND BAR, 1144 CD STRESS RELIEVED
STEEL ROUND BAR, 1144 CD STRESS RELIEVED
STEEL ROUND BAR, 1144 LASALLE STRESSPROOF CFS
STEEL ROUND BAR, 1144 LASALLE STRESSPROOF CFS
STEEL ROUND BAR, 1144 LASALLE STRESSPROOF CFS
STEEL ROUND BAR, 1144 LASALLE FATIGUEPROOF CFS
STEEL ROUND BAR, 12L14 LEDLOY CFS
STEEL ROUND BAR, 1215 CD
STEEL ROUND BAR, LASALLE ETD 150 CF
STEEL ROUND BAR, 4140 HFS AS-ROLLED
STEEL ROUND BAR, 4140 HFS ANNEALED
STEEL ROUND BAR, 4100, 4300, 9800 Q & T PER ASTM A434-90a CLASS BD
STEEL ROUND BAR, 4100, 4300, 9800 Q & T PER ASTM A434-90a CLASS BD
STEEL ROUND BAR, 4100, 4300, 9800 Q & T PER ASTM A434-90a CLASS BD
STEEL ROUND BAR, 4100, 4300, 9800 Q & T PER ASTM A434-90a CLASS BD
STEEL ROUND BAR, 4100, 4300, 9800 Q & T PER ASTM A434-90a CLASS BD
STEEL ROUND BAR, 8620 HFS AS-ROLLED
STEEL ROUND BAR, 8620 HFS ANNEALED
STEEL ROUND BAR, 8620 CDS ANNEALED
STEEL STAINLESS ROUND BAR, 303 HR ANNEALED
STEEL STAINLESS ROUND BAR, 303 CF
STEEL STAINLESS ROUND BAR, 303S HR ANNEALED
STEEL STAINLESS ROUND BAR, 303S CF
STEEL STAINLESS ROUND BAR, 303Se HR ANNEALED
STEEL STAINLESS ROUND BAR, 303Se CF
STEEL STAINLESS ROUND BAR, 304 HF TYPE A
STEEL STAINLESS ROUND BAR, 304 CF TYPE A
STEEL STAINLESS ROUND BAR, 304 TYPE A, CF
STEEL STAINLESS ROUND BAR, 316 HF TYPE A
STEEL STAINLESS ROUND BAR, 316 CF TYPE A
STEEL STAINLESS ROUND BAR, 316 CF TYPE A
STEEL STAINLESS ROUND BAR, AISI TYPE 329 ANNEALED
STEEL STAINLESS ROUND BAR, 416 TYPE A
STEEL STAINLESS ROUND BAR, 416 HEAT TREAT COND. T
STEEL STAINLESS ROUND BAR, 17-4 PH COND. H 1150 TYPE 630
STEEL STAINLESS ROUND BAR, 17-4 PH COND. A TYPE 630
STEEL STAINLESS ROUND BAR, 17-4 PH COND. H 900 TYPE 630


Material Properties are per ASTM specs when avalaible...

Pete
 
pdybeck,
I meant plain carbon graghite material. Used for bearings in the aerospace arena.

Chris,
Poco was the manufacture I dealt with in the past for carbon. my density might be off by little. Maybe make a generic material for this in the SW database.



Macduff [spin]
Colin Fitzpatrick
Mechanical Design Engineer
Solidworks 2007 SP 2.2
Dell 390 XP Pro SP 2
nVida Quadro FX 3450/4000



 
carbon schmarbon...

Pete
 
Thanks guys.
I could make diamond for carbon, but it's hard to do.[bigsmile]

Chris
SolidWorks 07 3.0/PDMWorks 07
AutoCAD 06
ctopher's home (updated 03-26-07)
 
Chris,
How about adding some density for Printed Wiring Boards like:

Premix Thermoplastics PRE-ELEC® ESD 4100=0.0343 lb/in³

I would like to hear from of the electrical folks out there. They might be more specific than us mechanical guys.

Macduff [spin]
Colin Fitzpatrick
Mechanical Design Engineer
Solidworks 2007 SP 2.2
Dell 390 XP Pro SP 2
nVida Quadro FX 3450/4000



 
I'll look into it. There are more than one mtl for PCB's. I will need to look more than just density.
Thanks.

Chris
SolidWorks 07 3.0/PDMWorks 07
AutoCAD 06
ctopher's home (updated 03-26-07)
 
Many materials for PCB's I imagine would be anisotropic (material response is dependent upon direction/orientation of a force relative to the material - think laminates/ply materials). You could not simply input a global modulus. You would need to define a modulus of elasticity for multiple directions/orientations. I think this is where some more serious FEA programs come into play. I think most of them come with some more serious libraries of materials and the ability to capture maerial properties for materials such as these. I mention this because the material database in SolidWorks is intended to work with Cosmos. I wonder if the material database can be carried over to a program like Cosmos Professional. Does the material database play nicely across those programs? Anyone in the know?

Pete
 
I have used these mtls in COSMOS and they worked well. Major aerospace companies and the US military bought into the FEA we did.

Chris
SolidWorks 07 3.0/PDMWorks 07
AutoCAD 06
ctopher's home (updated 03-26-07)
 
Chris, can the material database in basic SolidWorks "scale" up to cover these types of materials, or is it when you get into evaluating these types of materials/scenarios you just bag the solidworks material database and use a more extensive library. If the latter is the case, it would make more sense for us to submit an enhancement request for SolidWorks to set up the materials database to scale up to these situations so that we can put our time into adding material info to an animal that has the chance of being around for a while...

Pete
 
Pete,
I don't understand what you mean by "scale" up.
Thanks,

Chris
SolidWorks 07 3.0/PDMWorks 07
AutoCAD 06
ctopher's home (updated 03-26-07)
 
Lets say you spend all this time adding material info to the SolidWorks material database and it works great with solidWorks and Cosmos Designer. But lets say down the road you start using an FEA package that can analyze the materials that are anisotropic (laminates/plys/non-linear behaving materials). Can you still use the SolidWorks materials database that you spent all that time adding info to, or are you stuck re-creating all that information into another library/database that works with your more advanced FEA package. That is what I mean by scaling up...

Pete
 
With the database I created, I have been able to use it in COSMOSWorks & FloWorks without problems. I think it was up to SolidWorks 2005 we had to have a separate databse. Now, it's just one for all.
For a check, if anyone has CW or FW, please use the mtls and let me know how it works for you.
Thanks.

Chris
SolidWorks 07 3.0/PDMWorks 07
AutoCAD 06
ctopher's home (updated 03-26-07)
 
Chris,

Can CosmosWorks analyze materials that are anisotropic in nature? If so, does it just add fields to the SolidWorks material database? I haven't seen anything in the SolidWorks material database that shows this ability...

 
Status
Not open for further replies.

Part and Inventory Search

Sponsor