Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations GregLocock on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Material equivalent

Status
Not open for further replies.

avinodkumar

Mechanical
Mar 15, 2003
1
Can someone out there tell me the DIN equivalent of Alloy 20 ( ASTM A744 CN7M )?

avinodkumar
 
Replies continue below

Recommended for you

For castings I do not know but plate or pipe (ASTM 463/468/474) in Alloy 20 is called : NiCr20CuMo Werkstoff nr. 2.4660
 
I did not find any A 744 either
the only 700's I find for SAND cast alloys are
A713 & A771 which we pour both,
 
I've found a cross reference from CN-7M to Din 1.4500. I can't confirm how good it is, as I've not yet found a copy of the DIN spec. If I do I'll post it here.

Bruv
 
Found it. Din 1.4500 is not an exact match, but it's the nearest I could find. It is also known as GX7NiCrMoCuNb25-20.

Bruv
 
Got a reference from Allegheny Ludlum for Alloy 20 as DIN (2.4660).
 
I am trying to find an ASTM to DIN equivalent chart. Specifically, I am trying to identify the ASTM equivalent to DIN 1.7139. Please email me if you can help!
 
Maxrupert,

ASTM A 29 Standard Specification for Steel Bars, Carbon and Alloy, Hot-Wrought and Cold-Finished, General Requirements for lists the following grades that are close:

5115
C = 0.13-0.18
Si = 0.15-0.35
Mn = 0.70-0.90
Cr = 0.70-0.90

5120
C = 0.17-0.22
Si = 0.15-0.35
Mn = 0.70-0.90
Cr = 0.70-0.90

The DIN/EN grade 1.7139 has more Mn & Cr than either of these grades, so its hardenability will be higher than 5115. 5120 has slightly more carbon so it will be closer in hardenability, even with reduced Cr & Mn. Depending on your application, one of these grades or another alloy steel may be suitable.

Regarding equivalent steels & conversion among national & international standards, the following references are the best:

Worldwide Guide to Equivalent Irons and Steels, 4th Edition

Stahlschlüssel, 19th Edition
 