mechanodan
Automotive
- Dec 15, 2011
- 6
I would like to have some feedback on some material we are considering for half shafts in a custom car application.The app.is a shaft 24" long with a 1.2"spline journal diam.with 29 splines 45 degree pressure angle 24-48 pitch angle.The axle is exposed (visually)and I didn't want corrosion.I would also like to avoid any paint.Ford uses a necked down or waisted area of 1.437 down to the 1.2 spline diam.My concern is that if I make these shafts from 17-4 or 15-5 and use H-900 cond.Would it compromise the spline area in a torsional shock load? The parallel would be 4340 material which is used in the aftermarket and is presumably stronger than stock.