skengg
Mechanical
- Jun 19, 2021
- 133
Hello,
can anybody help to identify material grade just by material composition. i tried a lot but still couldn't be able to find exact grade.
carbon - 0.32% , silicone - 1.1% , manganese - 1.7% , chromium - 12.7%, molybdenum - 0.04%, Phosphorous - 0.02% , sulphur - 0.008%, nickel - less than 2%.
i checked major SS Grade but not matched with them.
i posted in this forum because this material used for ball manufacturing in ball valve.
can anybody help to identify material grade just by material composition. i tried a lot but still couldn't be able to find exact grade.
carbon - 0.32% , silicone - 1.1% , manganese - 1.7% , chromium - 12.7%, molybdenum - 0.04%, Phosphorous - 0.02% , sulphur - 0.008%, nickel - less than 2%.
i checked major SS Grade but not matched with them.
i posted in this forum because this material used for ball manufacturing in ball valve.