I am looking for material selection for flue gas cold stack for petroleum coke calcining plant. We use Mg(OH)2 slurry to reduce sulfur. The process conditions are as follows:
H2SO4 emissions 20 ppmvd upto 30 ppmvd.
O2 - 11.92%
chlorides - 350-500ppm coming from HCl from flue gas
- Flue gas contains magnesium-based particulate with particle sizes ranging from about 2 to 20µ.
Stack Height - 185ft
Bottom diameter - 7ft
stack temperature - 500F.
Dewpoint temperature of Sulfuric acid is 300-320 deg F.
It would be appreciated if someone could help me with the material selection.
H2SO4 emissions 20 ppmvd upto 30 ppmvd.
O2 - 11.92%
chlorides - 350-500ppm coming from HCl from flue gas
- Flue gas contains magnesium-based particulate with particle sizes ranging from about 2 to 20µ.
Stack Height - 185ft
Bottom diameter - 7ft
stack temperature - 500F.
Dewpoint temperature of Sulfuric acid is 300-320 deg F.
It would be appreciated if someone could help me with the material selection.