I have a project to reproduce rocker arms from early Fiat 4 cylinder OHV motors.

The ratio is 1.45:1, and the rocker will be fitted with a bronze bushing where it rides on the shaft. I have heard that EN8 (SAE 1049) or EN19 (SAE4140) could be used. In either case I would like to have the rocker body to have some ductility with the adjuster end and wear pad hardened for increased wear resistance.

Are there any other options?

Paul
 
Replies continue below

Recommended for you

EN19/4140 sounds like a good option to me. The whole part could be quenched and tempered to achieve a reasonable balance of strength and ductility, while the adjuster end and wear pad areas could be locally hardened by induction or flame in order to achieve a higher hardness surface zone. Q&T would probably be in the 32-39 HRC range, with surface hardness ~ 55-60 HRC after induction or flame heating.
 
There are many options, but likely you are limited by quantities. Are you making 10, 1000, 1 million? If it is either of the first two, then TVP gave you excellent advice. If it is the latter, then there are several other choices available.
 