sfifab
Structural
- Jan 30, 2012
- 6
I had a situation arise in our fabrication department where two galvanized channels are to be welded together using GMAW. Both pieces are .070" thickness, have a radius edge and when joined together produce a flare-v-grove. The parts are about 4' long, this groove runs the entire 4' length and normally, when broke correctly, produce a minimum root gap. Well today we have 50+ pieces that mate fine at the ends but produce an opposite bow in the middle leaving a 1/4" gap in the middle tapering to the ends. I have a quality guy telling our fab dept. to stick 1/16" shims in the gap, weld it up and take the shim back out. I know in my gut sticking shims in a gap so we don't have to scrap 50+ parts is not a good idea but, I can't find any evidence in the customer's spec or AWS D1.3.
Can anyone reference me to a specific clause?
Can anyone reference me to a specific clause?