Which is the maximum size possible of Flexible silica Aerogel Blanket - monolithic Aerogel (tranparent silica)?
 
Replies continue below

Recommended for you

for blanket, it can be made in 24" x 36" or 24" x 12'. the largest transparent aerogel made so far, by the swedeen (Airglass) is 53 x 53 cm2.
 