nikolastrojman
Industrial
- Jul 17, 2007
- 67
Hi!
Does anybody know how to determine the minimum yield strength for pipeline materials like e.g. L360 (or API 5L X52) above 60°C.
As per EN 1594, above 60°C min. yield strength should be corrected taking the temperature into consideration.
Does anybody know how to determine the minimum yield strength for pipeline materials like e.g. L360 (or API 5L X52) above 60°C.
As per EN 1594, above 60°C min. yield strength should be corrected taking the temperature into consideration.