Dear all,
At this time we are upgrading some of our seal systems from single to dual seal, mainly because of security improvements.
In applications of Hydrofluoric acid (HF) we have received proposals that specify a dual Type B seals (metal bellow)with plan API 53B.
Our experience in this applications is seal Type A with API plan 32/53B.
Some of you have experience with metal bellow seals in HF?
Advantages and disadvantages?
Can we to use only the API 53B without the API 32 plan?
At this time we are upgrading some of our seal systems from single to dual seal, mainly because of security improvements.
In applications of Hydrofluoric acid (HF) we have received proposals that specify a dual Type B seals (metal bellow)with plan API 53B.
Our experience in this applications is seal Type A with API plan 32/53B.
Some of you have experience with metal bellow seals in HF?
Advantages and disadvantages?
Can we to use only the API 53B without the API 32 plan?