I have th following composition of a metal sheet sample.
Mn : 0.068
Fe : 99.98
Cu : 0.114
Mo : 0.006

Anyone can help me with commerical grade number like (ASTM OR DN) to buy it commercially

Thanks in advance
Fayaz
 
Replies continue below

Recommended for you

Maybe he didn't have the equipment to measure the carbon or other low atomic number elements. I speculate that the percentage is of the measureable elements not the total mass or mole. Is it mass% or mole%?
 
Could this be vitreous enameling iron?