Hi everyone,
We are planning to use Methanol or Ethanol for cooling (-40ºC/-40ºF minimum temperature).
The problem we are facing (apart from the flammability) is the corrosion. We want to use aluminium pipes because of the good conductivity (copper is not possible for us).
How can we overcome this problem?
We could anodize the aluminium but we have some parts which are plates with holes for the coolant. We might also 3D print some tricky parts with the channels inside.
We could (if really needed) use steel or stainless steel
It seems the Ethanol is less corrosive, so in principle more promising, but also more expensive.
Does anyone have any knowledge about this topic?
Thank you in advance
Regards,
We are planning to use Methanol or Ethanol for cooling (-40ºC/-40ºF minimum temperature).
The problem we are facing (apart from the flammability) is the corrosion. We want to use aluminium pipes because of the good conductivity (copper is not possible for us).
How can we overcome this problem?
We could anodize the aluminium but we have some parts which are plates with holes for the coolant. We might also 3D print some tricky parts with the channels inside.
We could (if really needed) use steel or stainless steel
It seems the Ethanol is less corrosive, so in principle more promising, but also more expensive.
Does anyone have any knowledge about this topic?
Thank you in advance