Kholodov

Chemical
Oct 21, 2008
1
Hi,

I understand that there are some information regarding caustic scrubbers on this forum already, however, I can not find what I need.

I need to find Methyl Methacrylate vapour sollubility data (in Caustic sollution) for the design of the scrubber. I have not been able to locate anything usefull by searching the net.

If anyone could comment, would be much appreciated.
 
Replies continue below

Recommended for you

2 references
1) the handling and storage of acrylics esters from BASF;

2)Safe handling and storage of acrylic esters from EBAM ( european Basic Acrylic Monomer manufacturer association)

 
Dear Pierreick,

Where can I get the references?