I have a colleague that wants to install a micropile through an existing concrete slab. The slab is adequate for the pile loading. The procedure as follows:
Locate rebar,
Core drill the slab,
Install the micropile,
Mechanically roughen the sides of the core,
Clean the core using water and compressed air,
Install primer to the core sides,
Use Sikatop 123 Plus, with 3/8" aggregate added, to replace the concrete,
Bond strength is greater than or equal to the concrete strength (verify with Sika), and
The core 'plug' will support the reaction from the micropile.
Any comments or suggestions?
Locate rebar,
Core drill the slab,
Install the micropile,
Mechanically roughen the sides of the core,
Clean the core using water and compressed air,
Install primer to the core sides,
Use Sikatop 123 Plus, with 3/8" aggregate added, to replace the concrete,
Bond strength is greater than or equal to the concrete strength (verify with Sika), and
The core 'plug' will support the reaction from the micropile.