Mar 14, 2002 #1 jcole Mechanical May 18, 1999 6 CA I'm looking for a MIL-SPEC or standard that covers the application of: 1. High solids polyurethane topcoat 2. zinc chromate primer I have the standards that cover the type of primer and topcoat and the color, but I need something to cover the application. Thanks
I'm looking for a MIL-SPEC or standard that covers the application of: 1. High solids polyurethane topcoat 2. zinc chromate primer I have the standards that cover the type of primer and topcoat and the color, but I need something to cover the application. Thanks
Mar 15, 2002 #2 boo1 Mechanical Oct 31, 2001 2,129 US Try TT-P-2756A POLYURETHANE COATING: SELF-PRIMING TOPCOAT, LOW VOLATILE ORGANIC COMPOUNDS (VOC) CONTENT The Zinc Cromate has been canceled. Upvote 0 Downvote
Try TT-P-2756A POLYURETHANE COATING: SELF-PRIMING TOPCOAT, LOW VOLATILE ORGANIC COMPOUNDS (VOC) CONTENT The Zinc Cromate has been canceled.
Mar 27, 2002 #3 materialeng Aerospace Dec 15, 2001 1 IL for polyurethanr high solids the mil spec is mil-prf-85285 Upvote 0 Downvote