Does not appear that my attachment attached... I am trying again:
I have treated sheets of 16 gauge mild steel to produce results as attached in "Steel 1". What I used to achieve this result was to first wash the steel in Phosphoric acid. Leave for 3 hours, then wash with the blacking solution found at this page: - I am not sure what is in this... selenium dioxide maybe?
Later I have tried to reproduce these effects but have not been successful. Following the exact same steps I have only been able to produce the effect shown in "Steel 2". Any ideas what may be going on? The only thing that changed was the steel... I am using the same dealer but its not the same batch of steel- the first batch I bought months ago, the second recently. I can't seem to understand how that would make such a big difference. What I am most concerned about is the loss of the reds and blues... Any ideas out there.
I have treated sheets of 16 gauge mild steel to produce results as attached in "Steel 1". What I used to achieve this result was to first wash the steel in Phosphoric acid. Leave for 3 hours, then wash with the blacking solution found at this page: - I am not sure what is in this... selenium dioxide maybe?
Later I have tried to reproduce these effects but have not been successful. Following the exact same steps I have only been able to produce the effect shown in "Steel 2". Any ideas what may be going on? The only thing that changed was the steel... I am using the same dealer but its not the same batch of steel- the first batch I bought months ago, the second recently. I can't seem to understand how that would make such a big difference. What I am most concerned about is the loss of the reds and blues... Any ideas out there.