Hi

i need value of Ys for material sa-105 at 426 centigerade ... pls help me this is 166 or 165 mpa

Thanks
 
Replies continue below

Recommended for you

does it Really matter ?

"Hoffen wir mal, dass alles gut geht !"
General Paulus, Nov 1942, outside Stalingrad after the launch of Operation Uranus.
 
I'd be reviewing my load calcs and safety factors before caring about that last single MPa.
 
The sources that I would be checking would be the ASME codes I and IV dealing with the construction of process and heating boilers, respectively. Code VIII may also help as it deals with unfired pressure vessels.
 
Young's modulus may have more variation, which could have implications on support spacing - graph below for reference