I am trying to work out how a manufacturer put a ninety degree bend in a component 0.125” thick 2024-T42 with a bend radius of about 0.094”. The minimum bend radius charts give 0.250” when folded prior to heat treatment. This part is a flap bracket for a light aircraft and has not shown any cracking in service.
Also does any one know what are the minimum bend radius's for 6013-T4
Duncan
Also does any one know what are the minimum bend radius's for 6013-T4
Duncan