Dear Folks;
Could anyone tell me if there is a limit to wall thickness in aluminum extrusion using 6061-T6 ?
I have drawings of parts made in China with wall thickness 0.90mm and 0.80 +/- .15mm
I am being told that no one in North America can extrude sections of this thickness
Would appreciate any information that could be shared
Many Thanks in adviance
Adrian Dunevein