I have a Trumpf laser and I'm having problems cutting stainless, aluminum or anything reflective. The mirrors are buring out within hours. What am I doing wrong?

Thanks in advance for your help.
 
Replies continue below

Recommended for you

is the cooling system in order? Are the mirrors getting hot? Best check for water flow in the mirror mounts.


Chris Krug Maximum Up-time, Minimum BS
 
Could be output coupler or stressed lens too