[ul]
[li]AISI 410: corresponding to European X12Cr13 (W.-Nr. 1.4006), YM = 190 GPa @ 400 °C (limiting value for this steel).[/li]
[li]P91: 180 and 167 GPa respectively at 500 and 600 °C for the European equivalent X10CrMoVNb9-1 (W.-Nr. 1.4903).[/li]
[/ul]