Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Tek-Tips community for having the most helpful posts in the forums last week. Way to Go!

molecular sieve shelf life 2

Status
Not open for further replies.

tughanite

Industrial
Jul 18, 2003
4
0
0
MW
Hi,
Am doing a cost/benefit analysis of using molecular sieves versus azeotropic dehydration of ethanol. I would like to know how long it would take before I need to replace the adsorbent bed - in general
 
Replies continue below

Recommended for you

afaik, a general lifetime of 3-5 years (with continuous replacement of adsorbent loss) can be assumed. i have seen studies which expect a lifetime of 10 years, though i think this is too high a number as all adsorbent would have been exchanged due to losses in this timeframe.

hth,
chris
 