We have finish machined parts manufactured from 1/2"dia monel 400 bar. We have now found out that these parts have much more induced magnetism than we thought. The bars themselves are magnetic (I assume from the cold drawing process). The test reports show that the material has been stress relieved after straightening so I doubt whether a further stress relieve will help. Is there any way of demagnetizing these parts without a full solution anneal? I am afraid annealing may change the size of the parts.