1
- #1
motor rating: power=32kW, FLC=63A, Voltage=380V
before rewind: winding resistance=7.9ohms, line current=55A, phase current=31.8A
after rewind: winding resistance=9.1ohms, line current=84A, phase current=45A
after rewinding, the motor is drawing 33% more than the rated current but monitored it for 3days and it is not overheating. general consensus was, its specs will change after rewinding, so as long as its not overheating then its fine. my question is how do you determine the acceptable current and if this scenario can be left to run
before rewind: winding resistance=7.9ohms, line current=55A, phase current=31.8A
after rewind: winding resistance=9.1ohms, line current=84A, phase current=45A
after rewinding, the motor is drawing 33% more than the rated current but monitored it for 3days and it is not overheating. general consensus was, its specs will change after rewinding, so as long as its not overheating then its fine. my question is how do you determine the acceptable current and if this scenario can be left to run