Lahane
Mechanical
- Jul 23, 2010
- 27
One of my project requirement was to build a CS spool.NACE MR 0103 was involved in the specification
I already build a spool which has got a supporting PQR without pwht.As per NACE MR 0103, welding of p1 materials needs to be done as per RP0472.Road map of RP 0472 gives 3 options.one is pwht, second is chemistry control of base metal & last is HAZ hardness control in PQR as per sec 5.
Unfortunately, I have not follwed the first two option.
The last option says that practices to be followed in sec 5 should be specified by customer, but customer spec does not have such information.
What needs to be done to come out of this situation to comply with NACE requirement?
I already build a spool which has got a supporting PQR without pwht.As per NACE MR 0103, welding of p1 materials needs to be done as per RP0472.Road map of RP 0472 gives 3 options.one is pwht, second is chemistry control of base metal & last is HAZ hardness control in PQR as per sec 5.
Unfortunately, I have not follwed the first two option.
The last option says that practices to be followed in sec 5 should be specified by customer, but customer spec does not have such information.
What needs to be done to come out of this situation to comply with NACE requirement?