NACE vs. GP240GH+QT

Status
Not open for further replies.

adula29

Mechanical
Jul 10, 2009
53
Can we use GP240GH+QT as Killed carbon steel?
This is selection for pump casing for petroleum industry.
 
Replies continue below

Recommended for you

I don't know, what does the material standard or norm say about it?

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
GP240GH+QT is EN-10213-2

Chemical composition % of steel GP240GH (1.0619): EN 10213-2007
C Si Mn Ni P S Cr Mo V Cu
0.18 - 0.23 max 0.6 0.5 - 1.2 max 0.4 max 0.03 max 0.02 max 0.3 max 0.12 max 0.03 max 0.3
 
Steve and the rest,
There's been a rash of questions posted to incorrect forums recently.
I encourage users to manage their personal forum lists.
IM


"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor