I need to find a control valve that can resist wear from abrasive slurry.
Currently the 6"X8" angle valve that is used for the application wears out every 5 months. We have experimented with ceramic lined 10"X8" angle valves, but they are easily broken, and very expensive. One valve costs US$23,000.00. Clarkeson valves were also tried, but the rubber continued to be eroded and blocked the lines.
Currently the 6"X8" angle valve that is used for the application wears out every 5 months. We have experimented with ceramic lined 10"X8" angle valves, but they are easily broken, and very expensive. One valve costs US$23,000.00. Clarkeson valves were also tried, but the rubber continued to be eroded and blocked the lines.