I'm a Mechanical Engineer designing light hovercraft. We are using Polyethylene fuel tanks and have a hard time finding anything that sticks to Polyethylene very well.

We have been experiencing leaks around our fuel sending units and need a sealant that can stand up to constant contact of gasoline/oil and fumes (2-stroke). Most "fuel resistant" sealers just turn to mush or fall apart after a few days. And if they do hold up against the fuel/oil they often lose adhesion with the Polyethylene.

Any recommendations?
Thanks,

CS
 
Replies continue below

Recommended for you

You will not get anything to stick reliably. Use metal fittings and neoprene gaskets.
 
The old red Hermetite - if you can find it - and the newer Hylotyte Red are both fuel-resistant and semi-setting. They won't adhere but being semi-setting they may not need to. You'll need a reasonably accurate threaded fitting or flat sealing faces to achieve a good seal.


----------------------------------
image.php

If we learn from our mistakes I'm getting a great education!
 
1. Put all penetrations through the top of the tank.
2. Use a mechanical joint with a seal, e.g. an o-ring.

Spend a day in a junkyard. Look for plastic fuel tanks. Examine how they're mounted and how the connections are made.



Mike Halloran
Pembroke Pines, FL, USA
 
Another vote for a gasket or o-ring mechanical seal.

There are very few adhesives or sealants that stick to polyethylene.

If you can tolerate a "permenant" attachment, look at 3M DP-8500, although I'm not sure about its resistance to gas and oil.

If you need a removable-repairable attachment I doubt that you'll find anything suitable.
 
Mike...I like your advice about the junkyard. It's amazing how much you can learn from such escapades. Haven't done it in years...but should.
 