Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Need Mechanical and Chemical composition of BS material

Status
Not open for further replies.

samkor

Mechanical
Jan 3, 2011
5
KR
Dear All,
i need Mechanical and Chemical composition for BS1503-224.430N material.
reply would be highly appreciated.

Thanks
 
Replies continue below

Recommended for you

Samkor,

I believe, BS 1503:1989 has been WITHDRAWN & been replaced by BS EN 10222-1:1998, BS EN 10222-2:2000, BS EN 1022)

You may refer & check accordingly.
 

Carbon 0.20 max
Silicon 0.10 - 0.40
Manganese 0.80 / 1.40
Phos & Sulphur 0.040 max
Chromium 0.25 max
Molybdenum 0.10 max
Nickel 0.40 max
Copper 0.30 max
Niobium 0.01 - 0.06

Ni+Cr+Mo+cu = 0.80%

Supplied in various conditions.

Normalised, Normalised and Tempered - Tensile strength 430 - 550 N/mm2, Yield Strength 260 N/mm2 minimum, Elongation 19%, KV Impact 27 J minimum, limniting rulign section <=100 mm

Quenched and Tempered - Tensile strength 430 - 550 N/mm2, Yield Strength 245 N/mm2 minimum, Elongation 19%, KV Impact 27 J minimum, limniting rulign section >100 mm
 