May 3, 2011 #1 samkor Mechanical Jan 3, 2011 5 KR Dear All, i need Mechanical and Chemical composition for BS1503-224.430N material. reply would be highly appreciated. Thanks
Dear All, i need Mechanical and Chemical composition for BS1503-224.430N material. reply would be highly appreciated. Thanks
May 4, 2011 #2 ak1965 Mechanical Jul 28, 2007 158 IN Samkor, I believe, BS 1503:1989 has been WITHDRAWN & been replaced by BS EN 10222-1:1998, BS EN 10222-2:2000, BS EN 1022) You may refer & check accordingly. Upvote 0 Downvote
Samkor, I believe, BS 1503:1989 has been WITHDRAWN & been replaced by BS EN 10222-1:1998, BS EN 10222-2:2000, BS EN 1022) You may refer & check accordingly.
May 5, 2011 #3 59engineer Mechanical May 5, 2011 1 DE Please see here, there is an equivalence given. http://www.e-pipe.co.kr/eng/bs_no/bs_9.htmPerhaps this will help you. For the equivalence you will find the data here http://www.westyorkssteel.com/410.htmlhope this is sufficient Upvote 0 Downvote
Please see here, there is an equivalence given. http://www.e-pipe.co.kr/eng/bs_no/bs_9.htmPerhaps this will help you. For the equivalence you will find the data here http://www.westyorkssteel.com/410.htmlhope this is sufficient
May 16, 2011 #4 andyenergy Materials Feb 20, 2003 124 EU Carbon 0.20 max Silicon 0.10 - 0.40 Manganese 0.80 / 1.40 Phos & Sulphur 0.040 max Chromium 0.25 max Molybdenum 0.10 max Nickel 0.40 max Copper 0.30 max Niobium 0.01 - 0.06 Ni+Cr+Mo+cu = 0.80% Supplied in various conditions. Normalised, Normalised and Tempered - Tensile strength 430 - 550 N/mm2, Yield Strength 260 N/mm2 minimum, Elongation 19%, KV Impact 27 J minimum, limniting rulign section <=100 mm Quenched and Tempered - Tensile strength 430 - 550 N/mm2, Yield Strength 245 N/mm2 minimum, Elongation 19%, KV Impact 27 J minimum, limniting rulign section >100 mm Upvote 0 Downvote
Carbon 0.20 max Silicon 0.10 - 0.40 Manganese 0.80 / 1.40 Phos & Sulphur 0.040 max Chromium 0.25 max Molybdenum 0.10 max Nickel 0.40 max Copper 0.30 max Niobium 0.01 - 0.06 Ni+Cr+Mo+cu = 0.80% Supplied in various conditions. Normalised, Normalised and Tempered - Tensile strength 430 - 550 N/mm2, Yield Strength 260 N/mm2 minimum, Elongation 19%, KV Impact 27 J minimum, limniting rulign section <=100 mm Quenched and Tempered - Tensile strength 430 - 550 N/mm2, Yield Strength 245 N/mm2 minimum, Elongation 19%, KV Impact 27 J minimum, limniting rulign section >100 mm