I work with many different materials and was wondering if there is a good web site that gives the n & r values for many different materials for FEA. Right now I'm looking for 304SS that is half hard for the medical field.
 
Replies continue below

Recommended for you

If you need n and r values, then you should test some samples. Tensile testing costs around $100 per sample. What the he11 is the medical industry doing with all that money if they can't afford to pay for some simple testing?
 