I can find W-shapes and L-shapes. Does anyone know of a site where I can look sizes and properties for WT shapes?

Thanks.
 
Replies continue below

Recommended for you

AISC has the shapes posted in an excel worksheet. Go to aisc.org|free pubs. Under 'technical documents' click 'shapes database.' You'll find the whole kit and caboodle.
 
Thanks guys, I dont know why google wasn't turning up sites with WT shapes for me. I guess its Friday, and I am looking forward to Turkey next week.
 
Also, just keep in mind that a WT is usually just a Wide flange beam sliced in half. Therefore, if you've got the wide flange data, you have most of the properties already.
 