Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Neoprene Vs rubber as vibration isolation 1

Status
Not open for further replies.

marko333

Mechanical
Aug 6, 2003
21
Hi!

What the advantages and dis-advantages are in either fitting 'rubber' flexible connections to items of vibrating pant (ie pumps) or 'neoprene' (synthetic rubber) flexible connections.

Thank you.
 
Replies continue below

Recommended for you

Hello,

My experience with natural rubber is that it tends to age harden and is not as resistant to as many chemical solutions as is the neoprene material. Hope this helps.
 
I understand that rubber vibration isolations units are widely used as they offer a high degree of noise and vibration isolation. Is it the case that neoprene units are less effecient?
 
hello again,

I believe the rubber is used in vibration isolation units rather than neoprene because it is cheaper! As I said previously the neoprene has additives to improve chemical resistance which add to the cost.
 