Hey everyone!
So I'm designing this new building with quite heavily loaded RC columns (~800 kN design load) and the foundations are going to be placed close to the pre-existing ones that are also RC columns from the Soviet era from the 70s. I work with Eurocodes. Are there any methods that can help me determining the effect of the pre-existing columns' loads on the new foundations bearing capacity?
EDIT: The foundations are pads and not piles.
So I'm designing this new building with quite heavily loaded RC columns (~800 kN design load) and the foundations are going to be placed close to the pre-existing ones that are also RC columns from the Soviet era from the 70s. I work with Eurocodes. Are there any methods that can help me determining the effect of the pre-existing columns' loads on the new foundations bearing capacity?