We received a ready new 3-phase separator installed on a supporting skid.

We noticed that the insulation aluminum foils (cladding sheets) have black stains and possibly the aluminum layer has braded away due to bad transportation or storage.

These dark marks can not be cleaned by soap or water.

Could you advise on how best adjust the situation? or, shall it be kept as it is?

Please see the attached photo for more clarification.

Sincerely,
 
 https://files.engineering.com/getfile.aspx?folder=86e93956-d82d-4b46-87d6-1903d140a5ff&file=Aluminum_Cladding.docx
Replies continue below

Recommended for you

Is that insulation on the main vessel??

If so it's the best looking outer layer I've ever seen.

Aluminium creates it's own oxide layer, but it looks too "shiny" to me to be aluminium. Are you sure it isn't stainless?

how did that happen?

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
It is Aluminum sheets and it was reacted with a plastic cover during shipping and storage.
 