Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations cowski on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

New product to increase electrical contact

Status
Not open for further replies.
Replies continue below

Recommended for you

Try loading all these as images as you can get multiple images on a page otherwise no one will download all 7 images.

A bit more text or explanation would also help...

Remember - More details = better answers
Also: If you get a response it's polite to respond to it.
 
I got a little past 80% energy gain.
If a contact is so bad that the potential energy gain is so great, you need different, qualified installer.
Snake oil aside.
I have always had good luck with Penetroxtm.
It contains zinc particles to cut through the oxide layer, based in a grease to seal against air and moisture.
Good practice with aluminum is to wire brush the surface and immediately apply a coating of Penatrox.
Aluminum oxidizes almost immediately so the compound must be applied immediately after wire brushing, not after the coffee break.
Not for use on moving switch contacts due to the abrasive quality.
Screenshot_2023-08-14_at_13-29-34_BURNDY_P8A_Specsheet.pdf_cwpofy.png


[link Full Page of Specs][/url]

--------------------
Ohm's law
Not just a good idea;
It's the LAW!
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor