We have A312 317 12" 40S Pipe, Design Pressure of 2750 kpa and Design temps at 420C with a MDMT of -43C. We are trying to figure out if our WPS would require impact testing.
Table 323.2.2 4 States Austenitic stainless steels Note 6
(6) For austenitic stainless steels, impact testing is not required if the design minimum temperature is warmer than or equal to −104°C (−155°F),
and the stress ratio as defined in para. 323.2.2(b) is 0.3 or less. See also para. 323.2.2(g).
But I'm having a hard time trying to figure out what my Stress Ratio for this would be? Do we need Impact Testing?