Does anyone know the OD tolerance of NPS 4 SCH 80 pipe? Thank you.
 
Replies continue below

Recommended for you

Steel pipe, ASTM A53. Sorry for the omission.
 
outside diameter shall not vary by more than 1% of that specified.

4.5 x 0.01 = 0.045" max deviation from 4.5" o.d.
 