Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations IDS on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

OLIGOMER SEAL FAILURE

Status
Not open for further replies.

shyamshins

Mechanical
May 4, 2012
53
Dear Team,

We are facing seal failure in Oligomer application in Polymer plant below are process details :

Process Media : Oligomer ( Consists of Therapeutic acid, + Methyle Ethyle glycol )

Temperature : 261 Deg. Celcius.

Suction Presure : 5.9 Kg/cm2.

Discharge Pressure : 9 Kg/cm2

Viscosity : 257 mm2 / sec.

Attached is the seal failure photos.

Seal is of John Crane make 609 non cartridge seal.

Quench Media is Nitrogen.

Stationary face is fitted in pump stuffing box.

Seal fails every 6-7 months.

Kindly provide solution.
 