What are the possible cause of leaking of opzv batteries
I have battery bank with opzv 200 powersafe enersys.

 
Replies continue below

Recommended for you

Yes
Inspected , vapour leakage throuhh vent caps ,

Not through palatic jars or terminal seals,

But this vapour is colourless and once condensed become clear liquid in battery rack and battery surface the later yellowish stains

 
Is your charging voltage correct? Could it be too high?

-JFPE
 
It appears to be lead-acid technology, so the electrolyte is probably being boiled off.
 