Good day everyone. Would anyone know of a mill or distributor who handles STOCK sizes of oval or obround carbon steel (1020/1026) tubing. Let me eliminate 90% of your responses before-hand by saying that a custom run is out of the question, I only need a couple 100 feet of two sizes. Thanks for your input. Wes.
 
Replies continue below

Recommended for you

Have you tried searching under the term "elliptical tubing"?
 
heatseaker...

You might want to try running relatively thin-wall round [seamless] tubing thru oval rolling-dies [progressive sizing]. The Tubing can be formed cold, warm or hot[depending on severity of forming]... then stress-relieved If/as Required.

Good-luck

Note: in aviation "streamlined" [semi-oval] 4130 N steel is used for highly loaded struts.
 
Lock Joint Tube in Indiana carries quite a variety of ovals, along with other shapes.
 