Is it possible that the removal of a lubricating oil containing antioxidant additives may give rise to the nylon components within the system suffering oxidative attack. What i'm trying to say is........do the antioxidant additives in lubricant oil also act as an antioxidant film that protects components from oxidative attack..? Also, would the free radicals contributing to oxidation be neutralised by the additive , thus reducing potential for oxidative attack of the nylon components.