fareh
Structural
- Sep 30, 2008
- 19
Dears,
Would please explain how the Storage Tank underside is painted in accordance to API 650.
Background:
A steel welded tank with 18m dia and bottom plate thickness is 10 mm.
The Tank bottom underside spcs is as follow :
For Underside Tank
ABRASIVE BLAST CLEANING TO Sa 2.5
PRIMER AT SHOP 1 x 50 MICRON ZINC SILICATE
Mid Coat : 1 x 250 MICRON Coal tare epoxy
Final Coat : 1 x 250 MICRON Coal tare epoxy
Total Coat Thickness : 550 MICRON
Thanks,,
M. ALFAREH
Would please explain how the Storage Tank underside is painted in accordance to API 650.
Background:
A steel welded tank with 18m dia and bottom plate thickness is 10 mm.
The Tank bottom underside spcs is as follow :
For Underside Tank
ABRASIVE BLAST CLEANING TO Sa 2.5
PRIMER AT SHOP 1 x 50 MICRON ZINC SILICATE
Mid Coat : 1 x 250 MICRON Coal tare epoxy
Final Coat : 1 x 250 MICRON Coal tare epoxy
Total Coat Thickness : 550 MICRON
Thanks,,
M. ALFAREH