Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Tek-Tips community for having the most helpful posts in the forums last week. Way to Go!

Permedur 49 or Hiperco 50 bars pricing 1

Status
Not open for further replies.

israelkk

Aerospace
Dec 30, 2002
2,280
0
0
IL
Does anyone have a comparable prices per lb between low carbon alloys such as AISI 1010, 1020 compared to Permedur 49 or Hiperco 50 3" to 4" diameter bars. I do not need exact prices but a rough comparison.
 
Replies continue below

Recommended for you

I can't claim to know the source of the info, but my boss once handed me a torn, taped, and xeroxed chart that has relative costs of the soft magnetic materials we typically use. It goes like this:
[tt]
MATERIAL TYPE RELATIVE COST
Low Carbon Steel 0.5
Silicon Steel 1.0
Thin Electric Steel 10.0
49% Nickel (~Carpenter 49) 12.0
80% Nickel (~HyMu 80) 15.0
Cobalt Alloy (Hiperco 50) 35.0
[/tt]
 