Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations SSS148 on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Petcoke Gasification Refractory Reliability

Status
Not open for further replies.

PetroDDP

Petroleum
May 10, 2011
38
Limestone as CaCO3 and Fly ash (Coal Fly ash) are used as flux in Petcoke(High Vanadium content) Gasification unit under reducing atomsphere to minimise fusion temperature of petcoke. The fusion temperature is important as it affect the refractory life. Petcoke quality remains more or less consistent.So, to minimise Fusion temperature of petcoke what should be the Base/Acid ratio to operate gasifier at 1400 deg C ?
 