Contech2011
Civil/Environmental
I got shocker of my life to know the compressive strength @ 60 days of a 45 Mpa mix containing 35% replacement of cement with PFA (Type F C618) and about 5% of microsilica C1240, to be almost equal to 28 days strength. Only minor increase of 2 Mpa has occured @ 60 days.
I reckon the cause to be low reacting pozollonic activity of PFA. I doubt its Type F. Other factors may be temperature of the fresh concrete as casted...etc
Normally PFA concretes attain higher strengths @ later ages than early. I wait for 90 days test to one more set of the same batch.
Anybody can provide more insight on the above.
Thanks
I reckon the cause to be low reacting pozollonic activity of PFA. I doubt its Type F. Other factors may be temperature of the fresh concrete as casted...etc
Normally PFA concretes attain higher strengths @ later ages than early. I wait for 90 days test to one more set of the same batch.
Anybody can provide more insight on the above.
Thanks